PP vs ABS vs PC 材料比較:B2B ハードケース調達ガイド 2026
PP、ABS、PC は B2B 保護ケースの 3 大主要材料。PP が最軽量 + 最安価。ABS が中級。PC が最強 + 最高価。
材料特性比較
PP, ABS, and PC differ significantly in density, impact strength, temperature range, UV resistance, and chemical resistance. Material choice depends on application + spec requirements.
PP (polypropylene): density 0.90 g/cm³, lightest. Impact strength (Izod) 100-150 J/m. Temperature range -20C to +100C. UV resistance moderate (UV stabilizer required). Chemical resistance excellent (acids, bases, solvents). Tensile strength 25-40 MPa.
ABS (acrylonitrile butadiene styrene): density 1.04 g/cm³, mid-range. Impact strength 200-400 J/m. Temperature range -40C to +85C. UV resistance low (yellowing over time). Chemical resistance moderate. Tensile strength 35-50 MPa.
PC (polycarbonate): density 1.20 g/cm³, heaviest. Impact strength 600-900 J/m (highest). Temperature range -40C to +120C. UV resistance moderate (UV stabilizer required). Chemical resistance poor (solvents attack). Tensile strength 55-75 MPa.
PP+GF (glass fiber reinforced PP): density 1.05-1.20 g/cm³, mid-range. Impact strength 80-100 J/m (slightly lower than pure PP). Temperature range -30C to +110C. UV resistance moderate. Glass fiber content 10-30%.
コスト + MOQ + リードタイム
PP is cheapest, PC is most expensive. Cost difference affects B2B procurement decisions.
PP: USD 1.20-1.80/kg. Cheapest material. Easy to mold, low tool wear.
PP+GF (glass fiber): USD 1.50-2.50/kg. Mid-range. Higher strength than pure PP.
ABS: USD 1.80-2.50/kg. Mid-range. Common in consumer electronics.
PC: USD 3.00-5.00/kg. Most expensive. Specialty applications.
PP/PC blend: USD 2.50-3.50/kg. Mid-range. Combines PP + PC properties.
Tooling cost: PP tooling cheapest (lower temperatures, lower pressure). PC tooling most expensive (high temperatures, high pressure).
MOQ: PP 50-100 cases. ABS 100-200 cases. PC 200-500 cases (due to higher cost).
射出成形考慮事項
PP, ABS, PC differ significantly in injection molding parameters. Material choice affects tooling cost, cycle time, and product quality.
PP molding: melt temperature 200-260C, mold 20-30C, injection pressure 60-100 MPa. Cycle time 15-25 seconds. Easy to mold, low tool wear.
ABS molding: melt temperature 220-260C, mold 40-80C, injection pressure 70-100 MPa. Cycle time 20-30 seconds. Slightly more challenging than PP.
PC molding: melt temperature 280-320C, mold 80-120C, injection pressure 80-140 MPa. Cycle time 30-45 seconds. Requires precision tooling + high temperatures.
Tool wear: PP lowest (mild). ABS moderate. PC highest (abrasive + high temperature). PC tools require hardened steel (HRC 60+) and frequent maintenance.
Shrinkage: PP 1.5-2.5%. ABS 0.3-0.8%. PC 0.5-0.7%. PP requires more precise shrinkage compensation.
B2B アプリケーション推奨
Different B2B applications favor different materials. Below is the 2026 recommendation.
Photography / broadcast (camera cases): PP+GF for lightweight + adequate strength. PP+GF 30% for premium cases.
Military / tactical (NSN procurement): PP+GF for impact resistance + cost-effectiveness. Berry Amendment compliant materials.
Drone (1-5 kg payload): PP+GF for lightweight + impact resistance. Cost-effective for frequent replacement.
Medical (cleanability + compliance): ABS or PP for cleanability. Anti-microbial additive.
Industrial / measurement (5+ kg instrument): PP+GF for impact resistance + cost. Standard.
Aerospace (AS9100 + UL94 V-0): PC for strength + flame resistance. Premium cost.
Marine (IP68 + salt fog): PP or PP+GF for UV + salt water resistance.
Cold chain (2-8°C refrigerated): PP or PP+GF for low temperature toughness.
Consumer (camera / outdoor / Pelican alternative): ABS or PP for cost-effectiveness.
UV + 耐薬品性
UV and chemical resistance differ across PP, ABS, PC. Important for outdoor / industrial use.
UV resistance: PP moderate (UV stabilizer required for outdoor). ABS low (yellows over 6-12 months outdoor). PC moderate (UV stabilizer required for outdoor).
UV stabilizer additive: HALS (hindered amine light stabilizer) 0.5-1.5%. Carbon black 0.5-2% for black color. UV absorber 0.3-0.5% for transparent.
Chemical resistance: PP excellent (most acids, bases, solvents). ABS moderate (some solvents attack). PC poor (solvents like acetone, toluene attack).
Salt water: PP excellent (used for marine). ABS moderate. PC poor (becomes brittle).
Hydrocarbon (oil, gasoline): PP excellent. ABS moderate. PC poor (stress cracking).
Acid: PP excellent. ABS moderate. PC poor (concentrated acid attacks).
温度 + 機械的特性
Temperature range and mechanical properties are key for industrial / extreme environment cases.
Low temperature toughness: PP -20C, ABS -40C (better), PC -40C (best). For cold chain (-20C deployment), PC or ABS preferred over PP.
High temperature: PP 100C, ABS 85C, PC 120C. For hot industrial deployment (foundry, oven, etc.), PC preferred.
Tensile strength: PC 55-75 MPa (highest), ABS 35-50 MPa (mid), PP 25-40 MPa (lowest). For load-bearing applications, PC preferred.
Flexural modulus: PC 2300 MPa (highest stiffness), ABS 2000 MPa, PP 1500 MPa. For rigid cases, PC > ABS > PP.
Impact strength: PC 600-900 J/m (highest, including low temperature), ABS 200-400 J/m, PP 100-150 J/m. For impact-critical, PC > ABS > PP.
持続可能性 + リサイクル性
Sustainability and recyclability differ across PP, ABS, PC. Important for EU CSRD + US SEC ESG reporting.
PP recyclability: high. Mono-PP cases can be recycled as PP stream. Recycled PP (rPP) 30-50% blend available.
ABS recyclability: moderate. ABS recycling requires separation from other plastics. Mixed ABS quality issues.
PC recyclability: low. PC recycling requires separation from other plastics. Yellowing limits recycling cycles.
Carbon footprint: PP 1.5-2.5 kgCO2e/kg, ABS 3.0-4.0 kgCO2e/kg, PC 4.0-6.0 kgCO2e/kg. PP lowest carbon footprint.
EU CSRD + US SEC: Scope 3 supply chain emissions reporting. Recyclability data required.
B2B recommendation: PP or PP+GF for sustainable case procurement. Mono-PP design for end-of-life recyclability.
コスト最適化戦略
Material cost can be optimized by material choice, filler additives, and recycled content.
Use PP for cost-effective standard cases. 30-50% cost saving vs ABS or PC for non-critical applications.
Use PP+GF for premium cases with higher impact strength. Slightly higher cost vs pure PP.
Use ABS only when PP cannot meet spec (temperature, UV, impact). 30-50% cost premium vs PP.
Use PC only for extreme applications (aerospace, ultra-cold, ultra-high impact). 2-3x cost vs PP.
Recycled content: rPP 30-50% blend available. -5-15% cost vs virgin PP. Maintains 70-90% mechanical properties.
Calcium carbonate filler: 10-20% loading. -5-10% cost vs virgin PP. Slight property trade-off.
重要なポイント
- PP:USD 1.20-1.80/kg、最軽量、優れた耐薬品性
- ABS:USD 1.80-2.50/kg、中級、優れた低温靭性
- PC:USD 3.00-5.00/kg、最重量、最高耐衝撃性 + 温度範囲
- PP+GF:USD 1.50-2.50/kg、中級、ガラス繊維強化
- B2B デフォルト:ほとんどのケースは PP または PP+GF;低温用 ABS;航空宇宙用 PC
よくある質問
保護ケースに最適な材料は?
PP はほとんどの B2B 保護ケースのデフォルト最適材料。最軽量(0.90 g/cm³)、最安価(USD 1.20-1.80/kg)。
ケースには ABS とポリカーボネートのどちらがよいですか?
PC は耐衝撃性が高く、温度範囲が広い。しかし PC は ABS より 2-3 倍高い。
ケースは PP と ABS どちらが安いですか?
はい。PP は ABS より 30-50% 安い。
ガラス繊維強化 PP とは何ですか?
PP+GF(ガラス繊維強化ポリプロピレン)は、10-30% のガラス繊維を含む PP。
PP は UV 耐性がありますか?
PP は中程度の UV 耐性があります。UV 安定剤入りで 5-10 年屋外使用可能。
PP と PE プラスチックの違いは何ですか?
PP は融点が高く(160°C vs 130°C)、引張強度が高く、耐薬品性が優れています。
PP ケースはリサイクルできますか?
はい。PP ケースはリサイクル可能。モノ PP 設計は PP ストリームとしてリサイクル可能。